参考标准 Reference Standard ASTM A128 | 化学成分 Nominal Chemical Composition (W%) | 对应国际标准 Eqv. Standard GB5680 | |||||||
C | Mn | Cr | Mo | Ni | Si () | S () | P () | ||
A | 1.05-1.35 | ≥11.0 | - | - | - | 1.00 | 0.06 | 0.05 | GB 5680 ZGMn13-1 AS2074/H1A |
B-1 | 0.90-1.05 | 11.5-14.0 | - | - | - | 1.00 | 0.06 | 0.05 | GB 5680 ZGMn13-2 |
B-2 | 1.05-1.20 | 11.5-14.0 | - | - | - | 1.00 | 0.06 | 0.05 | GB 5680 ZGMn13-2,3 AS2074/H1A |
B-3 | 1.12-1.28 | 11.5-14.0 | - | - | - | 1.00 | 0.06 | 0.05 | GB 5680 ZGMn13-2,3 AS2074/H1A |
B-4 | 1.20-1.35 | 11.5-14.0 | - | - | - | 1.00 | 0.06 | 0.05 | GB 5680 ZGMn13-2,3 AS2074/H1A |
C | 1.05-1.35 | 11.5-14.0 | 1.50-2.50 | - | - | 1.00 | 0.06 | 0.05 | GB 5680 ZGMn13-4 AS2074/H1B |
D | 0.70-1.30 | 11.5-14.0 | - | - | 3.0-4.0 | 1.00 | 0.06 | 0.05 | - |
E-1 | 0.70-1.30 | 11.5-14.0 | - | 0.90-1.20 | - | 1.00 | 0.06 | 0.05 | GB 5680 ZGMn13-5 AS2074/H1C |
E-2 | 1.05-1.45 | 11.5-14.0 | - | 1.80-2.10 | - | 1.00 | 0.06 | 0.05 | GB 5680 ZGMn13-5 |
F | 1.05-1.35 | 6.0-8.0 | - | 0.90-1.20 | - | 1.00 | 0.06 | 0.05 | - |
- | 1.30-1.50 | ≥17.0 | - | - | - | 1.00 | 0.06 | 0.05 | AS2074/H1D |
性能 · 特点
产品性能
耐高温:1600℃
在渗碳,氮化,中性和氧化气氛中抗变形
缩短处理时间
更科学的工艺设计,使用寿命更长,安装效果更好
生产工艺:离心铸造工艺+精密铸造工艺+机械加工+焊接工艺
我们可以根据客户要求制造炉辊。
直径:50mm-1600mm; 长度:小于3m。
材料等级:750℃以下:Cr20Ni10;750〜850℃:Cr20Ni14;850〜950℃:Cr25Ni20Si2,SCH21;950〜1000℃:GX40NiCrSi38-18,1.4865;1000〜1100℃:GX40NiCrSiNb38-18,1.4849;1100〜1200℃:G-NiCr28W,2.4879。
产品特点
由不同材料制成的EB炉辊,例如不锈钢,Ni-Cr铁基耐热钢,用于工作温度高达1300℃的热处理炉。